No. |
Dimmension |
Zinc (ZnAICd) |
Aluminium (AlZnln) |
|||||
---|---|---|---|---|---|---|---|---|
|
I |
h |
a |
c |
Gross |
Nett |
Gross |
Nett |
1 |
400 |
40 |
125 |
460 |
10.50 |
9.95 |
4.00 |
3.45 |
2 |
450 |
40 |
125 |
510 |
12.00 |
11.35 |
5.00 |
4.35 |
3 |
550 |
45 |
125 |
610 |
16.00 |
15.25 |
6.50 |
5.75 |
4 |
650 |
45 |
125 |
710 |
21.00 |
20.10 |
8.00 |
7.10 |
5 |
800 |
50 |
125 |
860 |
27.00 |
25.95 |
11.50 |
10.45 |
5 |
900 |
50 |
125 |
960 |
30.00 |
28.80 |
1300 |
11.80 |
7 |
1200 |
50 |
125 |
1280 |
40.00 |
38.40 |
18 00 |
16.40 |
8 |
800 |
50 |
150 |
880 |
- |
- |
18 00 |
16.30 |
9 |
950 |
50 |
150 |
1030 |
- |
- |
21 00 |
19.20 |
10 |
1050 |
65 |
150 |
1130 |
- |
- |
30 00 |
27.60 |
11 |
1200 |
65 |
150 |
1280 |
- |
- |
34.00 |
31.60 |
Zinc anodes alloy
Alloying elements |
Maximum impurities |
Electrochemical parameters AZn |
|
---|---|---|---|
Al 0.12-0.18 |
Fe 0.005 |
Closed circuit potential accAg/AgCI |
1030 mV |
Cd 0.05-0 10 |
Pb 0.005 |
Consumption rate |
11.2 kg/A*yr |
Zn - balance |
Cu 0.002 |
Capacity |
780A*h/kg |
Sn 0.002 |
Aluminum anodes alloy
Alloying elements |
Maximum impurities |
Electrochemical parameters acc to DNV RP B401 test B (96H) |
|
---|---|---|---|
Zn 3 0-3.5 |
Fe 0.029-0.09 |
Closed circuit potential |
1090mV |
In 0.016-0.040 |
Si 0.034-0.10 |
Consumption Rate |
3.5 kg/A*r |
Al Remaining |
Cu 0.0011-0.005 |
Capacity |
2650A*h/kg |